Pipeline welding for the paper and cellulose industry

Location

Grums, Sweden

Technological pipeline welding work at the BillerudKorsnas Gruvon paper mill, using 111 welding process. The main materials: 1.4301, 1.4307, and 1.4432 with pipe diameters of DN25 to DN900 and wall thickness of 3.0 to 12.0 mm.